Fiberglass RV Door Skin Moisture Proof Scratch Resistant Stain Resistant Introduction When accounting for costs across the full service lifecycle, fiberglass RV door skins deliver distinct economic strengths. Their lightweight build lowers shipping and installation outlays, and excellent oxidation ...
Fiberglass RV door skin moisture proof
,FRP flat sheet scratch resistant
,Fiberglass RV door skin stain resistant
Fiberglass RV Door Skin Moisture Proof Scratch Resistant Stain Resistant
Introduction
Core Advantages

Application

|
|
|
|
|
FRP Flat Sheet Overview
Specialty FRP Flat Sheet:
FRP sheet performance data
No. |
Test ltems | Unit | 39140Series | 39380Series | 38501Series | 38351Series | Test Standard |
|---|---|---|---|---|---|---|---|
| 1 | Density | g/m3 | 1.35-1.5 | 1.35-1.55 | 1.4-1.6 | 1.5-1.8 | |
| 2 | Tensile Strenght | Mpа | 60-90 | 80-100 | 110-140 | 120-150 | GBT/T1447 |
| 3 | Flexural Strength | Mpa | 80-120 | 110-150 | 160-210 | 180-250 | GBT/T1449 |
| 4 | Flexural Modulus | Mpa | 4.1x10³-5.8x10³ | 4.6x10³-6.2x10³ | 5.5x10³-8.6x10³ | 5.3x10³-8.05x10³ | GBT/T1449 |
| 5 | Impact Toughness | KJ/m2 | 35-55 | 40-60 | 60-80 | 60-90 | GBT/T1451 |
| 6 | Water Absorbtion | % | 0.15-0.16 | 0.15-0.16 | 0.15-0.16 | 0.15-0.16 | GBT/T1462 |
| 7 | Oxygen Index | % | 22-32 | 22-32 | 22-32 | 22-38 | GBT/T8924 |
| 8 | Barcol hardness | Mg | 30-40 | 34-45 | 35-50 | 40-50 | GBT/T2576 |